    Abstract:

    A fast gelling process to synthesize kalsilite powder was performed by dropping aqua ammonia into the TEOS-KNO3-Al(NO3)3-EtOH-H2O system, which resulted in the formation of a gel in 5~12 minutes. Compared with the traditional sol-gel method, the gelation time is greatly shortened. The optimum gelling conditions are as follows: molar ratio of H2O to TEOS25, molar ratio of EtOH to TEOS4 and pH value about 9. Kalsilite powder is produced by treating the dried gel under 862℃ for 3 hours. The synthesized kalsilite particle is nearly 50 nm, and most of the secondary particles 5~20 μm. The specific surface area of synthesized kalsilite is 26.3 m2/g with an average intergranular pore size around 11.2 nm. The synthesized kalsilite powder is mesoporous with a bimodal pore distribution. Pure and homogeneous, stable in high temperature and with high potassium content and a bimodal pore distribution, the synthesized kalsilite powder can serve well as an efficient catalyst aid with relatively high application value.

    Reference
    Related
    Cited by
Get Citation

郑骥 马鸿文,2006,钾霞石快速溶胶-凝胶法制备及表征[J].岩石矿物学杂志,25(4):341~344. ZHENG Ji, MA Hong-wen,2006,Fast sol-gel synthesis and characterization of kalsilite[J]. Acta Petrologica et Mineralogica,25(4):341~344.

Copy
Share
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:November 04,2005
  • Revised:
  • Adopted:
  • Online:
  • Published:
Article QR Code